Atomic Layer Deposition Coated Polymer Films with Enhanced High-Temperature Dielectric Strength Suitable for Film Capacitors

Xudong Wu, Yichen Liu, Xiaotian Lin, Enling Huang, Guanghui Song, Daniel Q. Tan*

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

18 Scopus citations

Fingerprint

Dive into the research topics of 'Atomic Layer Deposition Coated Polymer Films with Enhanced High-Temperature Dielectric Strength Suitable for Film Capacitors'. Together they form a unique fingerprint.